DNV DH36

DNV DH40  DNV DH36  DNV DH36 

DNV DH36  shipbuilding  steel  plate  and  sheet

DNV DH36  Steel Description:
The steel for shipbuilding and oil platform---DH36, is the high tensile strength steel.
It is the Hull structural steel,with it's good toughness properties, higher strength,strong corrosion-resistance,the processing properties,and welding properties.

DNV DH36 Steel Application:
DNV DH36 steel can be used in the manufacture of the ocean ship's hull structure whose weight is above 10000 tons. DNV DH36 is mainly used to manufacture  the ship hull structure of ocean, coastal and inland sea areas , shipyards, oil platforms, pipelines in the ocean, coastal power plants, port facilities and other structural parts.

DNV DH36 Steel chemical composition by [%]:

Grade

C max

Si max

Mn

P max

S max

Als min

Ti max

Cu max

Cr
max

Ni
max

Mo
max

Nb

V

DNV DH36

0.18

0.50

0.90-1.60

0.035

0.035

0.015

0.02

0.35

0.20

0.40

0.08

0.02-0.05

0.05-0.10

Note: Generally speaking CE will be ≤ 0.40%. If the delivery condition is TMPC, the CE will be : ≤ 0.38% (thickness ≤ 50mm),≤0.40%( when the thickness >50-100).
Ceq% =(C+Mn)/6+(Cr+Mo+V)/5+(Ni+Cu)/15.

DNV DH36 Steel  Mechanical properties:

Grade

Rm (MPa)

Re(MPa) min

A% min

Akv/J min

DNV DH36

490-630

355

21

E.T °C

Thickness (mm)

-20

≤ 50

>50-70

>70-100

L

C

L

C

L

C

34

24

41

27

50

34

Note: In the list , Rm: .tensile strength,Re: Yield strength,A%: elongation, E.T: experimental temperature,L: lengthways, C: crosswise.

DNV DH36 Steel  Delivery state:

Grade

Fine grains elements

category

The thickness of steel

≤ 12

>12.5-20

>20-25

>25-35

>35-50

>50-100

DNV DH36

Nb+V or V

Plate/
sheet

A(50)

N(50),CR(50),TM(50)

N(50),CR(25),TM(50)

Profile steel

N(50),CR(50),TM(50),AR*(25)

-

Al or Al+Ti

Plate/
sheet

A(50)

AR*(25)

-

N(50),CR(50),TM(50)

N(50),CR(25),TM(50)

Profile steel

A(50)

N(50),CR(50),TM(50),AR*(25)

-

Note: 1. delivery condition: A =Any ; N=Normalized ; CR=Control Rolled ; TM=TMPC, Temperature - deformation control rolling; AR*= Can be hot rolled with the agreement of Classification Society ; CR*=Can be control rolled with the agreement of Classification Society .
2. The Figure in the ( ) means the sampling volume to do the impact test, the unit is Ton.(-) means without impact test.

Contrast in the different standard

ASTM A131M

TOCT 5521

BS LR

GB712

DH36

D36

DH36

D36

DNV DH36 shipbuilding plate has low alloy content, grain refinement elements like V, Ti, Nb, etc. Welding performance is superior. Preheating before welding is generally not proceeded, but it is done if it is at a low temperature or super thickness of structural components is welded,  that is , it needs to take preheating measures. Because this steel contains a small amount of V, Ti, Nb and other elements of grain refinement, and in order to reduce the hardening tendency of cracks to prevent cold(ing) crack, the use of welding wire energy may be more.

Source:

Tags:

Related Products
ADD:Headquarters Enterprise Base, Ruida Road,
Zhongyuan District, Zhengzhou City, 450000,China
TEL: 0086-371-86151827 ,0086-371-86151527
FAX: 0086-371-86011881
E-MAIL: [email protected]
Website : www.bebonchina.com
MESSAGE